Fabrication of a wound dressing mat based on Polyurethane/Polyacrylic acid containing Poloxamer for skin tissue engineering

Fabrication of a wound dressing mat based on Polyurethane/Polyacrylic acid containing Poloxamer for skin tissue engineering


چاپ صفحه
پژوهان
صفحه نخست سامانه
چکیده مقاله
چکیده مقاله
نویسندگان
نویسندگان
دانلود مقاله
دانلود مقاله
دانشگاه علوم پزشکی تبریز
دانشگاه علوم پزشکی تبریز

نویسندگان: مرجان قربانی , امیر عباس جلیلی بوالحسنی

کلمات کلیدی: Wound healing Polyurethane Polyacrylic acid Poloxamer Electrospinning nanofibers

نشریه: 7621 , 127891 , 633 , 2022

اطلاعات کلی مقاله
hide/show

نویسنده ثبت کننده مقاله مرجان قربانی
مرحله جاری مقاله تایید نهایی
دانشکده/مرکز مربوطه مرکز تحقیقات علوم تغذیه
کد مقاله 77444
عنوان فارسی مقاله Fabrication of a wound dressing mat based on Polyurethane/Polyacrylic acid containing Poloxamer for skin tissue engineering
عنوان لاتین مقاله Fabrication of a wound dressing mat based on Polyurethane/Polyacrylic acid containing Poloxamer for skin tissue engineering
ناشر 5
آیا مقاله از طرح تحقیقاتی و یا منتورشیپ استخراج شده است؟ بلی
عنوان نشریه (خارج از لیست فوق)
نوع مقاله Original Article
نحوه ایندکس شدن مقاله ایندکس شده سطح یک – ISI - Web of Science
آدرس لینک مقاله/ همایش در شبکه اینترنت

خلاصه مقاله
hide/show

Wound dressings are the main barrier between the wound area and the out environment. Here we design a novel electrospun nanofibers (NFs) based on polyurethane/polyacrylic acid/poloxamer (PU/PAA/POLO) as a biocompatible wound dressing. PU/PAA NFs with different weight concentration of POLO (5%, 10%, and 15%) were produced by electrospinning and the chemical structure, thermal stability, surface morphology, porosity, cytocompatibility, swelling and degradation ability, hydrophibicity and mechanical properties were investigated. Based on the obtained results, the PU/PAA/POLO fibers showed a uniform and beads-free morphology with acceptable mechanical characteristics. By increasing the weight concentration of POLO added to the NF struc- ture, an increase in the diameter of NFs (486.47 ±251.838 nm), swelling ratio (about 3%), wettability (51.59◦), and degradation degree (76%) were observed. Moreover, with increasing the diameter of NFs, the porosity (65.28 ± 0.9%), and WVTR (270.89 ± 3.01 g/m2.24 h) of NFs were significantly (P < 0.05) reduced. The MTT assay illustrated that produced NFs were non-toxic to the cells and the cell adhesion study showed that the developed NFs can form a good candidate platform for cell adhesion and proliferation. Based on these findings, it is expected that the produced PU/PAA/POLO NFs to be used as a wound dressing and accelerate the wound healing process.

نویسندگان
hide/show

نویسنده نفر چندم مقاله
مرجان قربانیپنجم
امیر عباس جلیلی بوالحسنیچهارم

لینک دانلود مقاله
hide/show

نام فایل تاریخ درج فایل اندازه فایل دانلود
Article.pdf1400/09/036345010دانلود