Bond Strength of White Mineral Trioxide Aggregate with and without Disodium Hydrogen Phosphate with Different Liquidto- Powder Ratios

Bond Strength of White Mineral Trioxide Aggregate with and without Disodium Hydrogen Phosphate with Different Liquidto- Powder Ratios


چاپ صفحه
پژوهان
صفحه نخست سامانه
چکیده مقاله
چکیده مقاله
نویسندگان
نویسندگان
دانلود مقاله
دانلود مقاله
دانشگاه علوم پزشکی تبریز
دانشگاه علوم پزشکی تبریز

نویسندگان: هادی مختاری زنوز , مهرداد لطفی , محمد فروغ ریحانی , آیدین سهرابی

کلمات کلیدی: Disodium Hydrogen Phosphate; Mineral Trioxide Aggregate; Push-Out Test; Root Canal Filling Materials; Root Canal Therapy

نشریه: 16512 , 3 , 12 , 2017

اطلاعات کلی مقاله
hide/show

نویسنده ثبت کننده مقاله هادی مختاری زنوز
مرحله جاری مقاله تایید نهایی
دانشکده/مرکز مربوطه دانشکده دندانپزشکی
کد مقاله 65440
عنوان فارسی مقاله Bond Strength of White Mineral Trioxide Aggregate with and without Disodium Hydrogen Phosphate with Different Liquidto- Powder Ratios
عنوان لاتین مقاله Bond Strength of White Mineral Trioxide Aggregate with and without Disodium Hydrogen Phosphate with Different Liquidto- Powder Ratios
ناشر 6
آیا مقاله از طرح تحقیقاتی و یا منتورشیپ استخراج شده است؟ بلی
عنوان نشریه (خارج از لیست فوق)
نوع مقاله Original Article
نحوه ایندکس شدن مقاله ایندکس شده سطح دو – PubMed
آدرس لینک مقاله/ همایش در شبکه اینترنت

خلاصه مقاله
hide/show

Mineral trioxide aggregate (MTA) can be used in the treatment of irritated vital pulp and repair of root perforations. However, the initial reaction of inflammatory cells to this material and also its setting time are not ideal. Studies have shown that disodium hydrogen phosphate (DHP), decreases the setting time of MTA, with no effect on its pH. This study was undertaken to evaluate the effect of DHP on push-out bond strength of MTA at different liquid-to-powder ratios. Methods and Materials: A total of 120 samples were prepared from the middle third of the roots of single-rooted teeth for evaluation of pushout bond strength. The push-out bond strength was measured in both groups after 72 h at different liquid-to-powder ratios, including 0.33:1, 0.5:1 and 0.6:1. Factorial ANOVA and Tukey’s HSD post-hoc tests were used to compare the differences between the independent groups. Statistical significant was set at P<0.05. Results: The push-out bond strengths of pure MTA and MTA+DHP groups were 10.96±5.78 and 13.32±5.03, respectively. Tukey’s HSD post-hoc test revealed significant differences between the two groups. Furthermore, there were no interactive effect between material and the liquid: powder ratio. Conclusion: Incorporation of DHP into MTA resulted in an increase in push-out bond strength of MTA, and an increase in liquid-to-powder ratio resulted in a decrease in push-out bond strength.

نویسندگان
hide/show

نویسنده نفر چندم مقاله
هادی مختاری زنوزاول
مهرداد لطفیچهارم
محمد فروغ ریحانیپنجم
آیدین سهرابیششم

لینک دانلود مقاله
hide/show

نام فایل تاریخ درج فایل اندازه فایل دانلود
15600-67184-1-PBmokhtari.pdf1397/10/04246039دانلود