Comparison of multiple rebond shear strengths of debonded brackets after preparation with sandblasting and CO2 laser.

Comparison of multiple rebond shear strengths of debonded brackets after preparation with sandblasting and CO2 laser.


چاپ صفحه
پژوهان
صفحه نخست سامانه
چکیده مقاله
چکیده مقاله
نویسندگان
نویسندگان
دانلود مقاله
دانلود مقاله
دانشگاه علوم پزشکی تبریز
دانشگاه علوم پزشکی تبریز

نویسندگان: مژگان کچوئی , سجاد شیرازی , امیر محمدی , سهند ریخته گران

کلمات کلیدی:

نشریه: 19913 , 3 , 10 , 2016

اطلاعات کلی مقاله
hide/show

نویسنده ثبت کننده مقاله سجاد شیرازی
مرحله جاری مقاله تایید نهایی
دانشکده/مرکز مربوطه مرکز تحقیقات لثه و دندان
کد مقاله 58850
عنوان فارسی مقاله Comparison of multiple rebond shear strengths of debonded brackets after preparation with sandblasting and CO2 laser.
عنوان لاتین مقاله Comparison of multiple rebond shear strengths of debonded brackets after preparation with sandblasting and CO2 laser.
ناشر 6
آیا مقاله از طرح تحقیقاتی و یا منتورشیپ استخراج شده است؟ بلی
عنوان نشریه (خارج از لیست فوق)
نوع مقاله Original Article
نحوه ایندکس شدن مقاله ایندکس شده سطح دو – PubMed
آدرس لینک مقاله/ همایش در شبکه اینترنت https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5025215/

خلاصه مقاله
hide/show

Background. Failure of orthodontic bracket bonds is a common occurrence during orthodontic treatment. Different techniques have been suggested in the literature to remove resin residues from the bracket bases and enamel surfaces to prepare the surfaces again after debonding. This study attempted to compare multiple rebond shear strengths (SBS) of debonded brackets following preparation with sandblasting and CO2 laser. Methods. The brackets were bonded on 30 human and bovine maxillary central incisors using self-curing composite resin. SBS was measured using Hounsfield testing machine. The brackets were rebonded for two other times after composite resin residues on their surfaces were removed, either with air abrasion or CO2 laser. The debonded brackets and enamel surfaces were also evaluated after each debonding procedure under a stereomicroscope in order to determine adhesive remnant index (ARI). SBS of debonded brackets after each step were compared between sandblast and CO2 laser groups. Results. We observed significant differences in SBS values between pre-recycling and first (P = 0.04), second (P = 0.007) and third recycling (P = 0.007) with laser. Recycling with sandblasting resulted in a decrease in SBS after the first and second recycling procedure; however, the SBS increased after the third recycling procedure, with no significant differences. Conclusion. SBS of brackets after recycling with sandblasting and laser beams was not significantly different, and both were at a favorable level. However, repeating the recycling procedure with sandblasting resulted in more favorable SBS compared to laser.

نویسندگان
hide/show

نویسنده نفر چندم مقاله
مژگان کچوئیاول
سجاد شیرازیششم
امیر محمدیدوم
سهند ریخته گرانچهارم

لینک دانلود مقاله
hide/show

نام فایل تاریخ درج فایل اندازه فایل دانلود
joddd-10-148.pdf1395/07/05254198دانلود